Extrusion Troubleshooting – Key Drivers (Part 3 of 3)

In plastics extrusion, troubleshooting is key to success, linking theory to practice and impacting the entire production process.
In plastics extrusion, troubleshooting is key to success, linking theory to practice and impacting the entire production process.

Extrusion troubleshooting draws the interconnection between the pillars of materials engineering, processing technology, and product development, bridging the gap between theory and praxis.

In plastics extrusion, troubleshooting emerges as the milestone of success, bridging the gap between theory and practice. Drawing from the pillars of materials engineering, processing technology, and product development, its significance reverberates throughout the manufacturing process. Mastery of these disciplines not only rectifies issues but fosters innovation, propelling the industry toward new heights of efficiency and excellence.

You can also read: Extrusion Troubleshooting – Key  Drivers (Part 2 of 3)

This set of commandments for extrusion troubleshooting offers a streamlined approach to diagnose and resolve common challenges, making them crucial for real-time problem-solving in diverse process settings However, it’s essential to recognize the specificity of each situation. By measuring as many variables as possible, we enhance our ability to analyze information and make informed decisions. Here we go with the last five topics:

Sharkskin

This defect is directly linked to the extruder die, raw material, and/or operational procedures. Remedial actions primarily involve elevating the melt and die temperatures, adjusting the resin gap, and opting for a lower modulus resin or one with a broader molecular weight distribution. Operational adjustments can also include changing mesh packs, reducing back pressure, and moderating extrusion speed.

Fisheye

Fisheye defects stem exclusively from raw material contamination or degradation. The recommended solutions comprise scrutinizing the screen pack for discolored material, indicating contamination from the hopper. Additionally, adhering to resin data sheet drying specifications is crucial. Finally, reducing temperatures, especially at the die, can mitigate cross-linking or gel formation.

Bubbles in the Product

Product bubbling typically arises from humidity or polymer resin degradation. Remediation strategies include resin drying as per manufacturer guidelines and conducting odor checks, if present, followed by adjusting melt temperatures accordingly.

Warped Part

Excessive shrinkage and warping often originate from the extruder die, cooling tank, or product design. Identifying the root causes entails adjustments such as aligning the spider mandrel concentrically with the extrusion die and ensuring uniform entry angle distribution. Aligning the cooling tank parallel to the extrusion outlet and detecting asymmetries and thickness variations can alleviate internal stresses.

Gel Formation

Gel formation, a byproduct of polymerization, extrusion, or contamination, demands meticulous attention. Effective measures include inspecting raw material for gel content, minimizing residence time in the extruder and screw, and employing low-coefficient friction coatings on screws and dies. Furthermore, using filters with high gel retention capacity and stringent contamination prevention and pre-production cleaning practices can avert such issues and their cascading effects.

You can also read: Plastic Extrusion Machine Market Size, Demand, Trends – 2032

By Andres Urbina | June 3, 2024

Share Your Thoughts

Your email address will not be published. Required fields are marked *

Stay updated
Each week, receive a summary of all the latest news from the world of Plastics
Choose Language